发明名称 |
High strength hardenable corrosion-resistant spring steel used for spring elements contains alloying additions of nickel, chromium, titanium and beryllium |
摘要 |
High strength hardenable corrosion-resistant spring steel consists of (in wt.%): 6.0-9.0 nickel, 11.0-15.0 chromium, 0.1-0.3 titanium, 0.2-0.3 beryllium, and a balance of iron. The steel has a martensitic temperature Ms of at least 130 deg C and a ferrite content of less than 3%. An Independent claim is also included for a process for the production of spring steel. Preferred Features: Up to 50% of the nickel content can be replaced by cobalt. Up to 35% of the chromium content can be replaced by molybdenum and/or tungsten.
|
申请公布号 |
DE10001650(A1) |
申请公布日期 |
2001.07.26 |
申请号 |
DE2000101650 |
申请日期 |
2000.01.17 |
申请人 |
VACUUMSCHMELZE GMBH |
发明人 |
WEBER, HARTWIN;DOERING, WALDEMAR;HAUSCH, GERNOT |
分类号 |
C21D6/00;C21D8/02;C21D9/02;C22C38/00;C22C38/44;C22C38/50;C22C38/52;(IPC1-7):C22C38/40 |
主分类号 |
C21D6/00 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|