ERHÖHEN DES MOLEKULARGEWICHTES VON POLYESTER UND FÜR DIESES VERFAHREN GEEIGNETE VORMISCHUNG
摘要
<p>An increase in the molecular weight of polyester and recycled polyester can be achieved by blending said polyester with a difunctional epoxy resin and a sterically hindered hydroxyphenylalkylphosphonic acid ester or half-ester and heating the blend to above the melting point (glass transition temperature) of the polyester.</p>