摘要 |
The cassette is characterized in that an ingredient having a glass fiber of 10~30% and unsaturated polyester resin of 70~90% are forming a proper cassette at such a situation that the original material of 20=F10% is thermally pressurized at approximately 130~150 deg. C for 1-2 minute. The cassette for medical use is characterized in that inside and outside of the cassette covered with urethane are plain to thereby be excellent in permeating rate and the degree of definition.
|