发明名称 アーク溶接方法
摘要 PROBLEM TO BE SOLVED: To perform arc welding to a base material while suppressing incomplete penetration and underfill height even when weld length is long or a shape is complicated.SOLUTION: An arc welding method includes: a first heating process S113 of generating a non-consumable electrode type arc 110 at a predetermined portion 101P on a weld part 101 to be welded to preheat a base material 100; a first welding process S116 of performing first consumable electrode type arc welding from the predetermined portion 101P toward one side in the extending direction of the weld part 101; a second heating process S163 of generating the non-consumable electrode type arc 110 at a predetermined portion 110P to reheat the base material 100; and a second welding process S166 of performing second consumable electrode type arc welding from the predetermined portion 110P toward the other side in the extending direction of the weld part 101.
申请公布号 JP6027483(B2) 申请公布日期 2016.11.16
申请号 JP20130085749 申请日期 2013.04.16
申请人 川崎重工業株式会社 发明人 松本 武志;安達 裕一朗;小林 篤央;上場 貴博;吉田 友祐
分类号 B23K9/173;B23K9/00;B23K9/23;B23K9/235 主分类号 B23K9/173
代理机构 代理人
主权项
地址