发明名称 |
誘電体セラミックス、誘電体セラミックスの製造方法及び積層セラミックコンデンサ |
摘要 |
A dielectric ceramic whose primary component is an ABO3 compound (A contains Ba and B contains Ti) has a per-layer thickness of approx. 0.5 μm or less, where the volume ratio to all dielectric sintered grains of those whose grain size is in a range of 0.02 μm to 0.15 μm is adjusted to a grain size distribution of 1% to 10%. High dielectric constant and high reliability can be achieved at the same time with the dielectric ceramic. |
申请公布号 |
JP5655036(B2) |
申请公布日期 |
2015.01.14 |
申请号 |
JP20120139801 |
申请日期 |
2012.06.21 |
申请人 |
太陽誘電株式会社 |
发明人 |
小西 幸宏;小和瀬 裕介;広井 一路;水野 高太郎;佐藤 歩 |
分类号 |
C04B35/468;H01B3/12;H01G4/12;H01G4/30 |
主分类号 |
C04B35/468 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|