摘要 |
PROBLEM TO BE SOLVED: To provide a container in which there is no possibility that a filling solid oily composition is rotated or released in the container when it is used. SOLUTION: In the container, the inner face is coated with a polymer with a glass transition temperature (Tg) in a range of -150°C to 10°C. A cosmetic article is obtained by filling the container with a solid oily cosmetic article. COPYRIGHT: (C)2009,JPO&INPIT |