发明名称 Fremgangsmåte ved sammenföyning av tofase rustfritt stål
摘要 In a method of bonding ferritic and austenitic dual stainless steels, an insert material made of a Ni base alloy having a melting point below 1290 DEG C is put between the bonding cross section faces of mother material steels comprising a dual phase stainless steel. A pressure force in the range of 3 MPa to 5 MPa is applied to the bonding area. The bonding area is heated to a temperature in the range of 1290 DEG C to the melting point of the mother material steel. The temperature is kept for a time in the range of 30 seconds to 180 seconds. <IMAGE>
申请公布号 NO983957(D0) 申请公布日期 1998.08.27
申请号 NO19980003957 申请日期 1998.08.27
申请人 DAIDO TOKUSHUKO KK 发明人 SHIMIZU, TAKAO;HORIO, HIROTSUGU;YAMAMOTO, NOBORU;INAGAKI, SHIGEYUKI;SUZUKI, HIROAKI;TSUCHIYA, MASAKI
分类号 H05B6/10;B23K20/00;B23K20/02;B23K20/14;B23K20/16;B23K101/06;C22C19/05;F28F21/08 主分类号 H05B6/10