发明名称 SINTERED STEEL MANUFACTURING PROCESS
摘要 According to the present invention, there is provided a microwave generator between the raw material feeding device and the ignition furnace of the Dwight Lloyd type sintering machine. (1) Microwaves alone heat a surface layer of raw material to 120 to 600 DEG C. (2) After the microwaves have heated the surface layer of raw material to 50 to 200 DEG C, a hot blast is sucked and the surface layer of raw material is heated to 150 to 600 DEG C. (3) Microwaves and the hot blast are simultaneously utilized so as to heat the upper layer of raw material to 150 to 600 DEG C. After the heating described in items (1), (2) and (3), the raw material is sintered. Due to the foregoing, the raw material is quickly dried, heated and sintered at high temperatures in a short period of time without the collapse of pseudo particles on the surface layer of raw material to be sintered, and sintered ore of high quality can be obtained. <IMAGE>
申请公布号 EP0767242(A4) 申请公布日期 1997.09.17
申请号 EP19950923548 申请日期 1995.06.29
申请人 NIPPON STEEL CORPORATION 发明人 HOSOTANI, YOHZOH;KONNO, NORIMITSU;NAKAI, HIROKI;UMEZU, AKIFUMI
分类号 C22B1/16;C22B1/20;F27B21/06;F27B21/08;F27D99/00 主分类号 C22B1/16
代理机构 代理人
主权项
地址