摘要 |
PCT No. PCT/SE95/01362 Sec. 371 Date Jun. 10, 1997 Sec. 102(e) Date Jun. 10, 1997 PCT Filed Nov. 16, 1995 PCT Pub. No. WO96/18676 PCT Pub. Date Jun. 20, 1996In a method of producing a suspension of a nonionic cellulose ether that has no turbidity point, the water forming part of the suspension is mixed with a dry mixture containing a cellulose ether, which is cross-linked with glyoxal, and an electrolyte salt. This electrolyte salt consists of a salt of a mixture of salts which, in water and at the concentration employed, results in a pH value below 8.0. Preferably, the cellulose ether is a hydroxyethylcellulose. |