发明名称 Cathode material and secondary battery using the same.
摘要 A cathode material made of anhydrous ferric sulfate with a hexagonal crystal structure is presented for use in a secondary battery which generates a stable open-circuit-voltage of about 3.6 volts and offers a recharge cycling capacity of over 100 times. The cathode material is obtained by heating hydrous iron sulfate material in a temperature range between 250 and 600 DEG C to remove the water of crystallization. The secondary battery made with this cathode material provides a long-service life and a stable output voltage economically, because the starting material, iron sulfate, is abundantly available at relatively low cost. <IMAGE>
申请公布号 EP0592301(A1) 申请公布日期 1994.04.13
申请号 EP19930402443 申请日期 1993.10.05
申请人 NIPPON TELEGRAPH AND TELEPHONE CORPORATION 发明人 OKADA, SHIGETO;OHTSUKA, HIDEAKI;ARAI, HAJIME;SHIBATA, MASASI;ICHIMURA, MASAHIRO
分类号 H01M4/58;H01M10/05 主分类号 H01M4/58
代理机构 代理人
主权项
地址