发明名称 |
Process for sealing an anodic coating obtained from a chromic acid bath. |
摘要 |
<p>To obtain simultaneously good corrosion resistance and good adhesiveness of the paint, the sealing of the oxide layer, obtained by chromic anodising, is performed under the following conditions: - bath composition: base: demineralised water, potassium or sodium dichromate: 8 to 12 grams per litre pH: adjusted to: 4.5 to 6.5 by a suitable addition of caustic soda. - bath temperature: 75 to 85 DEG C. - immersion time: sufficient to ensure a degree of hydration of the alumina coating of between 8 and 15 %. o</p> |
申请公布号 |
EP0545785(A1) |
申请公布日期 |
1993.06.09 |
申请号 |
EP19920403190 |
申请日期 |
1992.11.26 |
申请人 |
DASSAULT-AVIATION;SOCIETE DE GALVANOPLASTIE INDUSTRIELLE |
发明人 |
WOLF, ROBERT;BEVALOT, JEAN;BRAULT, CLAUDE |
分类号 |
C25D11/18 |
主分类号 |
C25D11/18 |
代理机构 |
|
代理人 |
|