UN PROCEDIMIENTO PARA OBTENER UNA ALEACION DE ALUMINIO QUE CONTIENE LITIO. |
摘要 |
<p>Aluminium alloys having compositions within the ranges (in wt %) 2 to 2.8 lithium-0.4 to 1 magnesium-1 to 1.5 copper-0 to 0.2 zirconium-0 to 0.5 manganese-0 to 0.5 nickel-0 to 0.5 chromium-balance aluminium. The alloys are precipitation hardenable and exhibit a range of properties, according to heat treatment, which make them suitable for engineering applications where light weight and high strength are required.</p> |
申请公布号 |
ES520100(D0) |
申请公布日期 |
1984.04.01 |
申请号 |
ES20000005201 |
申请日期 |
1983.02.25 |
申请人 |
THE SECRETARY OF STATE FOR DEFENCE IN HER BRITANNI |
发明人 |
|
分类号 |
C22C21/00;(IPC1-7):22C21/00 |