发明名称 PRODUCTION OF TILE EFFECTIVELY UTILIZING FUSED SLAG OF INCINERATION ASH
摘要 PROBLEM TO BE SOLVED: To effectively utilize refuse incineration ashes and to lower the firing temp. of tiles by press molding and drying a mixture composed of the fused slag of the refuse incineration ashes and clay minerals, then firing the moldings. SOLUTION: The refuse incineration ashes are heated and melted to 1150 to 1300 deg.C and are then pulverized to obtain the molten slag of the refuse incineration ashes. The dry body or slurry obtd. by mixing 30 to 95% molten slag of the refuse incineration ashes, 5 to 70% clay minerals, such as feldspar and pottery stone, having a grain size of <=100&mu;m and, if necessary, water is granulated to obtain the dry body for molding or granular powder for molding. The dry body for molding or granular powder for molding is press molded and is dried and the moldings are fired at 800 to 1150 deg.C.
申请公布号 JPH101357(A) 申请公布日期 1998.01.06
申请号 JP19960173002 申请日期 1996.06.11
申请人 TOKYO YOGYO CO LTD;KYOWA SEITO KK 发明人 YAMAMOTO KIMIJI;KATO NAOYUKI;HAYASHI SHIGERU
分类号 C04B33/135;C04B33/13;C04B35/00 主分类号 C04B33/135
代理机构 代理人
主权项
地址