发明名称 |
METHOD FOR PRODUCING SINTERED BODY |
摘要 |
PROBLEM TO BE SOLVED: To obtain a dense glass sintered body, because pores generated inside the sintered body not only causes strength decline of the sintered body but also causes scattering of light.SOLUTION: This method for producing a sintered body includes a step of forming a compact from glass powder by dry molding, a step of obtaining a precursor by sintering the compact, and a step of obtaining a sintered body by pressurizing and sintering the precursor under a mixed gas atmosphere containing oxygen; wherein the partial pressure of oxygen in the mixed gas is ≥10 vol.%. The relative density of the precursor is 90-96%, and the relative density becomes higher than the precursor by passing through pressurization sintering under the mixed gas atmosphere. |
申请公布号 |
JP2013173643(A) |
申请公布日期 |
2013.09.05 |
申请号 |
JP20120038761 |
申请日期 |
2012.02.24 |
申请人 |
SOPHIA SCHOOL CORP;CENTRAL GLASS CO LTD |
发明人 |
ITAYA SEIJI;ABE KAORI;TSUJI ATSUSHI;MIYAZAWA AKIMICHI |
分类号 |
C04B35/16;C03B19/06;G02B1/00 |
主分类号 |
C04B35/16 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|