摘要 |
<P>PROBLEM TO BE SOLVED: To provide a high conductivity conductor, and to provide a simple production method therefor. <P>SOLUTION: In the production method of a transparent conductor, a fluid dispersion for coating is prepared using the precipitation after centrifugal separation where the mass ratio of a dispersant (B) to carbon nano-tube (A)(content of (B)/content of (A)) is 0.5-3.0, produced by performing ultracentrifugal separation of a processed fluid dispersion containing the carbon nano-tube (A), the dispersant (B), and a dispersion medium (C) so that the mass ratio of a dispersant (B) to carbon nano-tube (A)(content of (B)/content of (A)) is 1.0-9.0 at a centrifugal acceleration of 100,000-200,000 G for 1-10 hours, and then the fluid dispersion for coating is applied onto a transparent base material and dried. A transparent conductor obtained by that method is also provided. <P>COPYRIGHT: (C)2013,JPO&INPIT |