<P>PROBLEM TO BE SOLVED: To provide a polyamide resin composition having high mechanical properties, particularly excellent rigidity and heat aging characteristics. <P>SOLUTION: The glass fiber reinforced polyamide resin composition includes 40-20 pts.wt. polyamide resin (A), 60-80 pts.wt. glass fibers (B), and 0.01-0.5 pt.wt. copper compound (C) and the average glass surface area (S) per unit number obtained from the remaining glass fiber length in a pellet composed of the resin composition is ≥1.1 times the critical glass surface area (Sc). <P>COPYRIGHT: (C)2012,JPO&INPIT |