发明名称 Silicon steel sheet and method thereof
摘要 A silicon steel sheet contains 0.01 wt. % or less C, 4 to 10 wt. % Si, 0.5 wt. % or less Mn, 0.01 wt. % or less P, 0.01 wt. % or less S, 0.2 wt. % or less sol. Al, 0.01 wt. % or less N, 0.02 wt. % or less O and the balance being Fe. The silicon steel sheet has grain boundaries and carbides which are precipitated on the grain boundaries. The carbides have an area of 20% or less to an area of the grain boundaries. The steel sheet is cooled at a cooling speed of 5° C./sec. or more in a temperature range of from 300 to 700° C.
申请公布号 US6241829(B1) 申请公布日期 2001.06.05
申请号 US19990457551 申请日期 1999.12.09
申请人 NKK CORPORATION 发明人 FUJITA KOICHIRO;TANAKA YASUSHI;NINOMIYA HIRONORI;HIRATANI TATSUHIKO;KASAI SHOJI
分类号 C23C10/08;C21D8/12;C22C38/00;C22C38/02;C22C38/06;C23C10/06;C23C10/60;H01F1/147;(IPC1-7):H01F1/04 主分类号 C23C10/08