PROBLEM TO BE SOLVED: To provide a molded article excellent in appearance such as luster molded from a resin composition which has high flowability, excellent moldability for a thin-wall article and excellent impact resistance, and a molded article which has also excellent frame retardance in addition to the above. SOLUTION: In a molded article molded from a resin composition comprising thermoplastic resins (A) and (B) which form at least two phase separation structures, at least two rubbery polymers (C) and (D) and, optionally, a flame retardant (E), the molded article has a morphology in which the distribution of the rubbery polymers formed after molding and solidification is such that 70-100 wt.% of rubbery polymer (C) is present in (A) and 0-30 wt.% of it in (B) and 70-100 wt.% of rubbery polymer (D) is present in (B) and 0-30 wt.% of it in (A).
|