发明名称 |
COPPER ALLOY MATERIAL FOR ELECTRICAL/ELECTRONIC PART AND PROCESS FOR PRODUCING THE SAME |
摘要 |
<p>A copper alloy material obtained by finish-rolling a material at a rate of work of 40% or lower, subjecting the finish-rolled material to a heat treatment with a continuous annealing furnace at a temperature of 500-800°C for 1-100 seconds, and subjecting the heat-treated material to a stress relieving treatment at a temperature of 400-600°C for 30-1,000 seconds. The copper alloy material for electrical/electronic parts underwent a dimensional change through the stress relieving treatment in the range of -0.02% to +0.02% in each of the directions parallel and perpendicular to the rolling direction.</p> |
申请公布号 |
WO2008044680(A1) |
申请公布日期 |
2008.04.17 |
申请号 |
WO2007JP69686 |
申请日期 |
2007.10.09 |
申请人 |
THE FURUKAWA ELECTRIC CO., LTD.;NAKANO, JUNSUKE;KITAZATO, KEISUKE;HIRAI, TAKAO |
发明人 |
NAKANO, JUNSUKE;KITAZATO, KEISUKE;HIRAI, TAKAO |
分类号 |
C22C9/06;B21B1/22;B21B3/00;C22F1/00;C22F1/08;H01B1/02;H01B5/02;H01B13/00 |
主分类号 |
C22C9/06 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|