摘要 |
<P>ON PREPARE DES COMPOSITIONS BITUME-POLYMERE EN MELANGEANT, ENTRE 130C ET 230C, UN BITUME AVEC UN COPOLYMERE DE STYRENE ET D'UN DIENE CONJUGUE ET UNE SOURCE DE SOUFRE, LE COPOLYMERE ET LA SOURCE DE SOUFRE ETANT AJOUTES AU BITUME SOIT DIRECTEMENT SOIT SOUS LA FORME D'UNE SOLUTION MERE DANS UNE HUILE HYDROCARBONEE, PUIS EN MAINTENANT LE TOUT SOUS AGITATION ENTRE 130C ET 230C PENDANT AU MOINS QUINZE MINUTES.</P><P>A TITRE DE SOURCE DE SOUFRE ON EMPLOIE 0,005 A 15 EN POIDS, PAR RAPPORT AU BITUME, D'UN OU PLUSIEURS POLYSULFURES LINEAIRES OU CYCLIQUES, POLYMERIQUES OU NON, ET NOTAMMENT DE PENTASULFURE DE DITERTIODODECYLE OU DE DINONYLE.</P><P>LES COMPOSITIONS BITUME-POLYMERE OBTENUES SONT UTILISABLES POUR LA REALISATION DE REVETEMENTS SUPERFICIELS ROUTIERS ET PRESENTENT UNE QUALITE CONSTANTE DE PROPRIETES.</P>
|