发明名称 PROCEDE DE SOUDAGE A L'ARC AVEC ELECTRODE CONSOMMABLE
摘要 <p>The method comprises performing welding cycles using transfer pulse and short-circuit, comprise moving an electrode at a velocity (V 1) during arcing period, and moving the electrode at a velocity (V p) during the transfer pulse welding cycle, where: the velocity (V p) is greater than the velocity (V 1); and the arcing period is followed by short-circuit period in which molten metal establishes a short-circuit with a molten bath. The method further comprises parametering the welding cycles using short-circuit and the welding cycles using transfer pulse. The method comprises performing welding cycles using transfer pulse and short-circuit, comprise moving an electrode at a velocity (V 1) during arcing period, and moving the electrode at a velocity (V p) during the transfer pulse welding cycle, where: the velocity (V p) is greater than the velocity (V 1); and the arcing period is followed by short-circuit period in which molten metal establishes a short-circuit with a molten bath. The method further comprises parametering the welding cycles using short-circuit and the welding cycles using transfer pulse according to the welding operation to be performed. The transfer pulsed welding cycles are sandwiched between the welding cycles by short circuit during the arcing period. The velocity (V p) of the movement of the electrode is constant. The welding cycle using transfer pulse comprises hot stage during which the electrode is supplied with a current having an intensity (I(H)) and a cold stage during which the electrode is supplied with a current having an intensity (I(B)) that is less than (I(H)), where the moving speed of the electrode varies between a value (V(PH)) during hot stage and a value (V(PB)) during the cold stage. The welding cycles using short-circuit comprise maintaining a supply current (I 2) of the consumable electrode during the arching period at the same time that the movement of the electrode at a velocity of (V 1), decreasing the intensity to reach a minimum intensity (I1), decreasing the velocity of the movement of the electrode to a value (V 3) during the short-circuit period, increasing the intensity during the short-circuit period to a value (V 4), and decreasing the intensity to reach I 1less than I 2. The intensity of the supply current varies according to a slope using the transfer pulsed welding cycle. An independent claim is included for an arc welding device.</p>
申请公布号 FR2977818(B1) 申请公布日期 2014.05.23
申请号 FR20110056257 申请日期 2011.07.11
申请人 AIR LIQUIDE WELDING FRANCE;L'AIR LIQUIDE,SOCIETE ANONYME POUR L'ETUDE ET L'EXPLOITATION DES PROCEDES GEORGES CLAUDE 发明人 BURVELLE NICOLAS;CHEVALIER RICHARD;PLANCKAERT JEAN-PIERRE;PLOTTIER GERARD
分类号 B23K9/173 主分类号 B23K9/173
代理机构 代理人
主权项
地址