摘要 |
PROBLEM TO BE SOLVED: To provide a woody plate having anti-allergenicity, which is excellent in a scratch resistance, abrasion resistance, and gloss change resistance and does not need repair with wax.SOLUTION: The woody plate having the anti-allergenicity has a plate-shaped woody base material and a functional layer which is arranged on the surface of the woody base material and formed from a single layer or a plurality of layers, and a layer constituting the surface of the functional layer contains an anti-allergenic agent. The layer constituting the surface of the functional layer is a coating film at least 5 μm in thickness which is formed by applying/curing a curable resin composition containing the anti-allergenic agent, an aliphatic urethane acrylate resin having an average molecular weight (Mw) of 500-2,000 and at least three (meth)acryloyl groups, and α-alumina powder having an average particle size of 1-10 μm and/or resin beads having an average particle size of 3-30 μm as a reinforcement filler. |