摘要 |
Cobalt-base superalloys having special utility in the production of industrial gas turbine hot gas path components because of their unique combination of properties including excellent hot corrosion resistance, creep rupture strength at high temperature, metallurgical stability, tensile ductility and weldability, consist essentially of 0.3 to 0.6% carbon, 27-35% chromium, 9-16% nickel, 6-9% tungsten, 0.45 to 2.0% tantalum, up to 3.0% hafnium, up to 0.1% columbium, up to 0.7% zirconium, not more than 2.0% iron, 1.5% manganese and silicon and 0.05% boron, balance cobalt, the carbide formers being selected to satisfy the following equation: <MATH> |