发明名称 PREPARATION OF PITCH FOR CARBON MATERIAL
摘要 PURPOSE:To obtain pitch useful for preparing especially carbon fiber, having a low softening point and improved spinnable properties, by using a heavy oil obtained by fluid catalytic cracking of petroleum, etc. and a residual oil fraction of hydrogenation product of petroleum heavy oil as raw materials. CONSTITUTION:A mixture of (A) a heavy oil having >=200 deg.C boiling point obtained by fluid catalytic cracking or thermal cracking and (B) a residual oil fraction of a formed oil obtained by hydrogenating a petroleum heavy oil is heat-treated at 350-450 deg.C (preferably at 380-420 deg.C), to give pitch usually containing 30-80wt% mesophase, from which pitch substantially containing 100wt% mesophase is separated. A heavy oil having 200-450 deg.C boiling point among a reaction product obtained by fluid catalytic cracking of gas oil, normal-pressure residual oil, etc. in the presence of a silica alumina catalyst, etc. at 450-550 deg.C may be cited as the component A.
申请公布号 JPS6036594(A) 申请公布日期 1985.02.25
申请号 JP19830144404 申请日期 1983.08.09
申请人 IDEMITSU KOSAN KK 发明人 NISHITANI HIROSHI;SUGIOKA YASUSHI
分类号 C01B31/00;C01B31/02;C10C3/02;C10C3/10;D01F9/14;D01F9/155 主分类号 C01B31/00
代理机构 代理人
主权项
地址