摘要 |
The present invention provides a thin container production method capable of forming a thin container having a thickness of about 0.7 mm by injecting a molten resin of a polylactic acid into a narrow cavity. The production method according to the present invention produces a thin container W having a thickness in a range of 0.3 to 0.7 mm by injection molding of a polylactic acid resin. The molten resin of the polylactic acid impregnated with supercritical carbon dioxide in a range of 0.5 to 2.5 percent by mass relative to the total amount is injected into a cavity 29 corresponding to the thin container W. |