发明名称 Super-clean steel
摘要 The steel of the present invention satisfies the following requirement for non-metallic inclusion area: when the steel is melted by an electron beam under the conditions of an irradiation rate of 200 to 600 J/sec., an irradeation time of 10 to 25 seconds, and an irradeation energy of 5000 J or more, the area of non-metallic inclusions existing in the surface of the sample after solidification falls within 15,000 mum2 or less. The steel exhibits excellent cold workability and fatigue properties.
申请公布号 US6402858(B1) 申请公布日期 2002.06.11
申请号 US20000527571 申请日期 2000.03.16
申请人 SUMITOMO METAL INDUSTRIES, LTD. 发明人 ISHIZAKA YUKIO
分类号 C21D8/06;C22C38/02;C22C38/04;C22C38/18;C22C38/42;C22C38/44;C22C38/46;(IPC1-7):C22C38/18;C22C38/32;C22C38/40 主分类号 C21D8/06
代理机构 代理人
主权项
地址