摘要 |
An Eu-activated &bgr;-sialon phosphor showing a high luminance, the use thereof and the method of producing the same. The &bgr;-sialon phosphor includes, as a matrix, a &bgr;-sialon crystal represented by a general formula: Si6-zAlzOzN8-z (0<z<4.2), wherein Eu, which serves as an activator, is solid-soluted in the &bgr;-sialon crystal, and the ratio of Eu2+/(Eu2++Eu3+) is 0.8 or more. It is preferred that the amount of Eu in the solid solution is 0.1 to 1 mass % with respect to the mass of the &bgr;-sialon crystal.
|