摘要 |
PROBLEM TO BE SOLVED: To obtain a current carrying slide body superior in heat resistance/ electroconductivity/lubricity. SOLUTION: This is that which is coated with a greasy lubricant 25 composed of 20 to 30 wt.% graphite whose average particle size is from 5 to 30μm and 70 to 80 wt.% perfluoropolyether 22 whose viscosity is from 200 to 350 so that the film thickness becomes 10μm or more.
|