<p>This invention provides a ferromagnetic shape memory alloy comprising 25 to 50 atomic% of Mn, 5 to 18 atomic% in total of at least one metal selected from the group consisting of In, Sn and Sb, and 0.1 to 15 atomic% of Co and/or Fe with the balance consisting of Ni and unavoidable impurities. The ferromagnetic shape memory alloy has excellent shape memory properties in a practical temperature region and causes a magnetic field induced reverse transformation in a practical temperature region, whereby the magnetism is changed and the shape is recovered.</p>
申请公布号
WO2007001009(A1)
申请公布日期
2007.01.04
申请号
WO2006JP312835
申请日期
2006.06.27
申请人
JAPAN SCIENCE AND TECHNOLOGY AGENCY;ISHIDA, KIYOHITO;OIKAWA, KATSUNARI;KAINUMA, RYOSUKE;KANOMATA, TAKESHI;SUTOU, YUJI