发明名称 Extrusion bonded laminates for absorbent articles
摘要 Absorbent articles in which the outer cover has an extrusion bonded laminate.
申请公布号 US9169384(B2) 申请公布日期 2015.10.27
申请号 US201213431026 申请日期 2012.03.27
申请人 The Procter & Gamble Company 发明人 Autran Jean-Philippe Marie;Muslet Iyad;Bland David G.;Cancio Leopoldo V.;Neton Janet;Mansfield Todd Leon
分类号 A61F13/514;B32B27/12;C08L53/02;A61F13/15;A61F13/49;B32B25/10;B32B27/32;C08L23/08;C08L23/14;C08L23/16;C08L53/00;B32B5/02;B32B5/06;B32B5/08;B32B5/26;B32B7/12;B32B25/04;B32B25/08;B32B25/12;B32B25/16;B32B25/18;B32B27/08;B32B27/20;B32B27/22;B32B27/28;B32B27/30;B32B27/34;B32B27/36;C08L23/06;C08L23/12 主分类号 A61F13/514
代理机构 代理人 Carter Kathleen Y.
主权项 1. An absorbent article comprising: a topsheet; an outer cover; an absorbent core disposed between the topsheet and outer cover; wherein the outer cover comprises an extrusion bonded laminate, the extrusion bonded laminate comprising: a multi-layer coextruded elastomeric film, comprising a core layer, a first outer layer, and a second outer layer, wherein the core layer is between the first and second outer layers; a nonwoven consisting of fibers and/or filaments;wherein the first outer layer is non-adhesively joined to the nonwoven via extrusion coating, such that the first outer layer is a tie layer between the core layer and the nonwoven;wherein the second outer layer is non-adhesively joined to the core layer, such that the second outer layer is a skin layer;wherein the first and second outer layers comprise polyolefin elastomers (POEs);wherein the first and second outer layers comprise a blend of two ethylene rich copolymers, wherein ethylene is between 10% and 97%;wherein the extrusion bonded laminate is mechanically activated using intermeshing gears;wherein the outer cover is elastic at 50% engineering strain; wherein the nonwoven has a high chemical affinity for the first outer layer; wherein the first outer layer has a low chemical affinity for the core layer; and wherein the multi-layer coextruded elastomeric film has a basis weight from 1 gsm to 25 gsm; and wherein the level of stretch of the activated laminate (% engineering strain at 1 N/cm force, as measured by the tensile test) is about 62% to about 144%.
地址 Cincinnati OH US