摘要 |
<p>Disclosed is a thermoplastic elastomer composition which contains a thermoplastic elastomer having a melting point of 200-300ºC, the thermoplastic elastomer being obtained by mixing starting materials comprising a (meth)acrylic elastomer and a cyclic polyester oligomer in a weight ratio of 40/60 to 95/5 [((meth)acrylic elastomer)/(cyclic polyester oligomer)], with heating at a temperature of 120-300ºC. Also provided are a process for producing the thermoplastic elastomer composition and a molded object obtained by heating and molding the composition. The thermoplastic elastomer composition is usable in sealing materials, packings, vibration-damping members, tubes, automotive parts, electrical/electronic components, etc.</p> |