发明名称 METHOD FOR MANUFACTURING POSITIVE ACTIVE MATERIAL AND POSITIVE ACTIVE MATERIAL
摘要 <P>PROBLEM TO BE SOLVED: To suppress gas evolution in a nonaqueous electrolyte secondary battery. <P>SOLUTION: A positive active material is manufactured by coating composite oxide particles mainly comprising lithium nicklate with a silicate compound and then conducting heat treatment. In the secondary battery using the positive active material manufactured in the process and having a carbonate ion content of 0.15 wt.% of less, gas evolution in the battery can be suppressed. The heat treatment is conducted at 300-1,200&deg;C. As the silicate compound, colloidal silica is preferably used, 100 pts.wt. composite oxide particles are coated with 0.01-5.0 pts.wt. silicate compound, and heat treatment is conducted. <P>COPYRIGHT: (C)2010,JPO&INPIT
申请公布号 JP2010129470(A) 申请公布日期 2010.06.10
申请号 JP20080305201 申请日期 2008.11.28
申请人 SONY CORP 发明人 WATANABE HARUO;OYAMA YUUDAI;AZUMA HIDETO;FUJITA SHIGERU
分类号 H01M4/525;H01M4/36;H01M4/62 主分类号 H01M4/525
代理机构 代理人