发明名称 SURFACE-TREATMENT METHOD FOR TIN-PLATED DRAWN AND IRONED CANS
摘要 <p>A surface which has excellent adhesivity to paint, good corrosion resistance, and low friction may be obtained on drawn and iron tin plated cans by spraying the can surface for a time between 5 and 60 seconds at a temperature between 40 and 60 °C with an aqueous treating liquid having a pH between 4 and 6 and comprising (i) orthophosphoric acid and/or condensed phosphoric acids and (ii) a concentration of at least 0.1 w/o of a water soluble oligomer according to general formula (I) wherein n is a number with a value between 10 and 30 and each of X and Y independently represents hydrogen or a group Z, wherein Z has a chemical composition conforming to general formula (II) wherein each of R1 and R2 is an alkyl or hydroxyalkyl group having from 1 to 5 carbon atoms, except that at least 25 % of the total of all the X and Y groups in the oligomer are Z rather than hydrogen; and drying the surface thus sprayed, optionally after having first rinsed the sprayed surface with water.</p>
申请公布号 WO1991010756(A1) 申请公布日期 1991.07.25
申请号 US1991000202 申请日期 1991.01.10
申请人 发明人
分类号 主分类号
代理机构 代理人
主权项
地址